MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chase Plastics CP Pryme® NN102MD Nylon 6/6, 2% Molybdenum Disulfide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, MoS2 Filled

Material Notes: Nylon 6/6, 2% Molybdenum Disulfide Lubricated Pellets.

Information provided by Chase Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccDry; ISO 1183
Water Absorption 2.3 %
@Temperature 22.8 °C
Dry polymer after 50%RH.; ISO 62
 8.5 %
@Temperature 22.8 °C
Dry; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 8700 psiConditioned; ISO 527-2
 13800 psiDry; ISO 527-2
Elongation at Break 10 %Dry; ISO 527-2
 25 %Conditioned; ISO 527-2
Elongation at Yield 3.5 %Dry; ISO 527-2
 20 %Conditioned; ISO 527-2
Tensile Modulus 220000 psiConditioned; ISO 527-2
 520000 psiDry; ISO 527-2
Charpy Impact, Notched 2.20 ft-lb/in²
@Temperature 22.8 °C
Dry; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 446 °FDry. Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 185 °FDry. Unannealed; ISO 75-2/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHA924 / 268575

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.