MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sumitomo Chemical Sumipex® BF3 Acrylic Resin, GP Blow Molding Grade
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product Characteristics

  • Excellent Weatherability
  • High Transparency
  • Good Heat Resistance

Information provided by Calsak Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 95ASTM D785
Tensile Strength, Yield 10000 psi
@Thickness 3.17 mm
Type I; ASTM D638
Elongation at Break 7.0 %ASTM D638
Flexural Yield Strength 16000 psi
@Thickness 3.17 mm
Type I; ASTM D790
Flexural Modulus 450000 psi
@Thickness 3.17 mm
Type I; ASTM D790
Izod Impact, Notched 0.790 ft-lb/in
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 201 °F
@Thickness 3.17 mm
annealed; ASTM D648
Vicat Softening Point 219 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Haze <= 0.50 %ASTM D1003
Transmission, Visible 93 %Total light Transmission; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Chemical Sumipex® LG Acrylic Resin, High Flow
Sumitomo Chemical Sumipex® MH Acrylic Resin, Heat Resistant
Envalior Akulon® K240-HP PA6-I, Conditioned, Heat Stabilized, Impact Modified, Extrusion Blow Molding
Lucky EH-910 Acrylic, Extrusion Grade
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer

PLBZ79 / 50548

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.