System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6 (PA6), 40% Glass/Mineral Reinforced, Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Glass/Mineral Reinforced
Material Notes:
PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.48
g/cc
ISO 1183
Linear Mold Shrinkage, Flow
0.0043
cm/cm
150x105x3; ISO 2577
0.0051
cm/cm
60x60x2; ISO 2577
Linear Mold Shrinkage, Transverse
0.0067
cm/cm
60x60x2; ISO 2577
0.0108
cm/cm
150x105x3; ISO 2577
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
213
MPa
ISO 2093-1
Tensile Strength at Break
120
MPa
5 mm/min; ISO 527-1,-2
Elongation at Break
2.8 %
5 mm/min; ISO 527-1,-2
Tensile Modulus
8000
MPa
1 mm/min; ISO 527-1,-2
Flexural Strength
193
MPa
2 mm/min; ISO 178-A
Flexural Yield Strength
193
MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus
7500
MPa
2 mm/min; ISO 178-A
Flexural Strain at Break
3.6 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO)
35.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1U
35.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched
40.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1U
45.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Electrical Properties
Original Value
Comments
Comparative Tracking Index
425
V
Solution A; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
40.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow
80.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point
221
°C
10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi)
190
°C
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
215
°C
ISO 75-1,-2
Deflection Temperature at 8.0 MPa
80.0
°C
ISO 75-1,-2
Vicat Softening Point
215
°C
@Load 5.10 kg
120°C/h; ISO 306
Flammability, UL94
HB
@Thickness 0.750 mm
Shrinkage, MD
0.060 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction 150x105x3; ISO 2577
0.17 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction; 60x60x2; ISO 2577
Shrinkage, TD
0.060 %
@Treatment Temp. 120 °C,
Time 14400 sec
150x105x3; ISO 2577
0.15 %
@Treatment Temp. 120 °C,
Time 14400 sec
60x60x2; ISO 2577
Processing Properties
Original Value
Comments
Melt Temperature
290
°C
Mold Temperature
80.0
°C
Back Pressure
50.0
-
60.0
MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Eurotec® Tecomid® NB40 KK40 NL PA6, 40% glass fiber/mineral reinforced, natural
Envalior Durethan® BM 40 X H3.0 EF 000000 Nylon 6 (PA6), 40% Glass/Mineral Filled, Dry
Envalior Durethan® BM 40 X H2.0 EF 900116 Nylon 6 (PA6), 40% Glass/Mineral Filled, Dry
Envalior Durethan® BM 40 X H2.0 EF 900116 Nylon 6 (PA6), 40% Glass/Mineral Filled, Conditioned
Envalior Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6 (PA6), 40% Glass/Mineral Reinforced, Conditioned
PLANW9524 / 208289
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.