MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
Special Metals NIMONIC® Alloy 90
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: A precipitation-hardenable nickel-chromium-cobalt alloy having high stress-rupture strength and creep resistance at temperatures to about 1700°F (920°C). The alloy also has good resistance to high-temperature corrosion and oxidation. Used for blades and discs in gas turbines, hot-working tools, and springs. Standard product forms are round, flats, extruded section, plate, sheet, strip, tube, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: Nickel-Chromium Alloy; UNS N07090; BS 3075 (NA19), HR2, HR202, HR402, HR501 - HR503; Werkstoff Nr. 2.4632; AMS 5829, WL Nr. 2.4632; AFNOR NCK 20 D; AECMA Pr EN 2295 - 2299, 2400, 2401, 2412, 2669, 2670
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.18 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1030 MPa
@Temperature 550 °C
Precipitation Hardened prior to test
 1150 MPa
@Temperature 23.0 °C
Tensile Strength, Yield 725 MPa
@Strain 0.2 %
Precipitation Hardened. Value at room temperature
 690 MPa
@Strain 0.2 %,
Temperature 550 °C
Precipitation Hardened prior to test
Elongation at Break 30 %Precipitation Hardened
 25 %
@Temperature 550 °C
Precipitation Hardened prior to test.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000118 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.7 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.446 J/g-°C
Thermal Conductivity 11.5 W/m-K
Melting Point 1310 - 1370 °C
Solidus 1310 °C
Liquidus 1370 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 1.0 - 2.0 %
Boron, B <= 0.020 %
Carbon, C <= 0.13 %
Chromium, Cr 18 - 21 %
Cobalt, Co 15 - 21 %
Copper, Cu <= 0.20 %
Iron, Fe <= 1.5 %
Manganese, Mn <= 1.0 %
Nickel, Ni 55 %As remainder
Silicon, Si <= 1.0 %
Sulfur, S <= 0.015 %
Titanium, Ti 2.0 - 3.0 %
Zirconium, Zr <= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 718
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened
Special Metals INCONEL® Alloy X-750
Special Metals NIMONIC® Alloy 80A
Universal Wire Works Nimonic 90 (AMS 5829) Filler Metal

NINC64 / 17414

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.