System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
ExxonMobil LD 317.09 Film Resin
(discontinued **)
Categories:
Polymer
;
Film
;
Thermoplastic
;
Ethylene Vinyl Acetate
;
Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Material Notes:
LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.
Information provided by ExxonMobil Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.925
g/cc
ExxonMobil Method
Vinyl Acetate Content
6.1 %
ExxonMobil Method
Thickness
2.00
mil
Melt Flow
0.25
g/10 min
ExxonMobil Method
Mechanical Properties
Original Value
Comments
Film Tensile Strength at Yield, MD
1270
psi
at 2% offset; ASTM D882
Film Tensile Strength at Yield, TD
1080
psi
at 2% offset; ASTM D882
Film Elongation at Break, MD
150 %
ASTM D882
Film Elongation at Break, TD
550 %
ASTM D882
Film Elongation at Yield, MD
7.5 %
ASTM D882
Film Elongation at Yield, TD
5.5 %
ASTM D882
Elmendorf Tear Strength, MD
80.0
g/mil
ASTM D1922
Elmendorf Tear Strength, TD
120
g/mil
ASTM D1922
Dart Drop
220
g/mil
ASTM D1709
Film Tensile Strength at Break, MD
3800
psi
ASTM D882
Film Tensile Strength at Break, TD
3900
psi
ASTM D882
1% Secant Modulus, MD
20000
psi
ASTM D882
1% Secant Modulus, TD
23400
psi
ASTM D882
Thermal Properties
Original Value
Comments
Melting Point
216
°F
Peak Melting Temperature; ExxonMobil Method
Optical Properties
Original Value
Comments
Haze
12 %
ASTM D1003
Gloss
54 %
45°; ASTM D2457
Descriptive Properties
Features
Thermal Stabilizer
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Versalis Greenflex® FD 50 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Dow Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
ExxonMobil LD 141.87 Shrink Film Resin
ExxonMobil Escorene™ UL 00112 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ UL 00018 Ethylene Vinyl Acetate Copolymer (European Grade)
PEXB015 / 37320
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.