MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
304 Stainless Steel (UNS S30400); Annealed Bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Tensile property data reported is typical longitudinal.

Austenitic Cr-Ni stainless steel. Better corrosion resistance than Type 302. High ductility, excellent drawing, forming, and spinning properties. Essentially non-magnetic, becomes slightly magnetic when cold worked. Low carbon content means less carbide precipitation in the heat-affected zone during welding and a lower susceptibility to intergranular corrosion.

Applications: beer kegs, bellows, chemical equipment, coal hopper linings, cooking equipment, cooling coils, cryogenic vessels, dairy equipment, evaporators, flatware utensils, feedwater tubing, flexible metal hose, food processing equipment, hospital surgical equipment, hypodermic needles, kitchen sinks, marine equipment and fasteners, nuclear vessels, oil well filter screens, refrigeration equipment, paper industry, pots and pans, pressure vessels, sanitary fittings, valves, shipping drums, spinning, still tubes, textile dyeing equipment, tubing.

Corrosion Resistance: resists most oxidizing acids and salt spray.

UNS S30400; AMS 5501, 5513, 5560, 5565; ASME SA182, SA194 (8), SA213, SA240; ASTM A167, A182, A193, A194

Key Words: aisi304, AISI 304, T304, T 304, SUS304, SS304, 304SS, 304 SS, UNS S30400, AMS 5501, AMS 5513, AMS 5560, AMS 5565, AMS 5566, AMS 5567, AMS 5639, AMS 5697, ASME SA182, ASME SA194 (8), ASME SA213, ASME SA240, ASME SA249, ASME SA312, ASME SA320 (B8), ASME SA358, ASME SA376, ASME SA403, ASME SA409, ASME SA430, ASME SA479, ASME SA688, ASTM A167, ASTM A182, ASTM A193, ASTM A194, ASTM A666, FED QQ-S-763, MILSPEC MIL-S-5059, SAE 30304, DIN 1.4301, X5CrNi189, B.S. 304 S 15, EN 58E, PN 86020 (Poland), OH18N9, ISO 4954 X5CrNi189E, ISO 683/13 11, 18-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 640 MPa
@Temperature 24.0 °C
 640 MPa
@Temperature 24.0 °C
 1150 MPa
@Temperature -78.0 °C
 1150 MPa
@Temperature -78.0 °C
 1520 MPa
@Temperature -196 °C
 1520 MPa
@Temperature -196 °C
 1720 MPa
@Temperature -269 °C
 1720 MPa
@Temperature -269 °C
 1860 MPa
@Temperature -253 °C
 1860 MPa
@Temperature -253 °C
Tensile Strength, Yield 235 MPa
@Temperature 24.0 °C
 235 MPa
@Temperature 24.0 °C
 280 MPa
@Temperature -196 °C
 280 MPa
@Temperature -196 °C
 300 MPa
@Temperature -78.0 °C
 300 MPa
@Temperature -78.0 °C
 400 MPa
@Temperature -269 °C
 400 MPa
@Temperature -269 °C
 420 MPa
@Temperature -253 °C
 420 MPa
@Temperature -253 °C
Elongation at Break 27 %
@Temperature -253 °C
 27 %
@Temperature -253 °C
 30 %
@Temperature -269 °C
 30 %
@Temperature -269 °C
 45 %
@Temperature -196 °C
 45 %
@Temperature -196 °C
 50 %
@Temperature -78.0 °C
 50 %
@Temperature -78.0 °C
 76 %
@Temperature 24.0 °C
 76 %
@Temperature 24.0 °C
Reduction of Area 54 %
@Temperature -253 °C
 54 %
@Temperature -253 °C
 55 %
@Temperature -269 °C
 55 %
@Temperature -269 °C
 66 %
@Temperature -196 °C
 66 %
@Temperature -196 °C
 76 %
@Temperature -78.0 °C
 76 %
@Temperature -78.0 °C
 82 %
@Temperature 24.0 °C
 82 %
@Temperature 24.0 °C
Modulus of Elasticity 193 GPa
Notched Tensile Strength 710 MPa
@Temperature 24.0 °C
 710 MPa
@Temperature 24.0 °C
 1060 MPa
@Temperature -196 °C
 1060 MPa
@Temperature -196 °C
 1120 MPa
@Temperature -253 °C
 1120 MPa
@Temperature -253 °C
Poissons Ratio 0.29
Shear Modulus 77.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
@Temperature 20.0 °C
 0.000116 ohm-cm
@Temperature 650 °C
Magnetic Permeability 1.020at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.3 µm/m-°C
@Temperature 0.000 - 100 °C
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
 18.4 µm/m-°C
@Temperature 0.000 - 538 °C
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.2 W/m-K
@Temperature 0.000 - 100 °C
 21.5 W/m-K
@Temperature 500 °C
Melting Point 1400 - 1455 °C
Solidus 1400 °C
Liquidus 1455 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 18 - 20 %
Iron, Fe 66.345 - 74 %As remainder
Manganese, Mn <= 2.0 %
Nickel, Ni 8.0 - 10.5 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
316 Stainless Steel, annealed bar
304 Stainless Steel
303 Stainless Steel, annealed bar
Titanium Ti-6Al-4V (Grade 5), Annealed
304 Stainless Steel (UNS S30400); Cold Finished and Annealed Bar

MQ304A18 / 151040

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.