Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized. Available as natural and several colors powder compounds. High quality Polyethylene recommended for general purpose applications. Frequently used for water tanks and small to medium size containers exhibiting very good mechanical properties. When used for inner layers, it provides excellent smooth finish and texture. Natural Resin, which is used as a carrier in color compounds meets all requirements of US food and drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact. Information provided by Polimeros Mexicanos |
Recommended for water tanks and small to medium size containers |