MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Alfa Chemistry Materials Scandium Metal
Categories: Metal

Material Notes: Scandium Metal is applied in various superalloys which show excellent metallic performance with their light gravity. The main application of Scandium by weight is in Scandium-Aluminum alloys for minor aerospace industry components. They were used in the Russian military aircraft, specifically the MiG-21 and MiG-29. Some items of sports equipment, which rely on high performance materials, have been made with Scandium-Aluminum alloys. Employed in solid state synthesis of unusual clusters, Sc19Br28Z4, (Z=Mn, Fe, Ru or Os). These clusters are of interest for their structure and magnetic properties. A much more abundant element on the sun than on earth, scandium is still widely distributed on earth, occurring in over 800 mineral species. Scandium is a silvery-white metal that develops a yellow or pink tint when exposed to air. It is relatively soft and is chemically similar to the rare earth metals. Fairly stable in air Ductility Good

Applications: it increase the strengths of alloys of metals such as chromium, aluminum, and magnesium. Scandium Metal can be further processed to various shapes of ingots, pieces, wires, foils, slabs, rods, discs and powder.

Molecular Formula: Sc

IUPAC Name: scandium

Room temperature, sealedAlfa Chemistry Materials product group: Metal

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.985 g/cc
Molecular Weight 45 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 1540 °C
Boiling Point 2830 °C
 
Descriptive Properties
AppearanceSilvery
CAS Number7440-20-2
Purity99.999%99.999% 99.99% 99.9%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

ZZALFA66584 / 304827

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.