MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Surlyn® 8945 Thermoplastic Ionomer Resin
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Molded

Material Notes: Surlyn® 8945 provides high flow properties and consistent, easy processing in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the ionomer spectrum.

Surlyn® 8945 is ideal for applications where fast molding cycles at reduced molding temperatures are desired. The high flow characteristics also facilitate molding in thin sections. Surlyn® 8945 provides good cut resistance and high resiliency, particularly when used in blends with different cations, such as with surly® 9945.

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D792
Melt Index of Compound 4.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength at Break 22.1 MPaASTM D638
Tensile Strength, Yield 15.9 MPaASTM D638
Elongation at Break 330 %ASTM D638
Flexural Modulus 0.448 GPaASTM D790(B)
 
Thermal PropertiesOriginal ValueComments
Melting Point 47.0 - 88.0 °CASTM D3418(DSC)
Vicat Softening Point 71.0 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Surlyn® 9945 Thermoplastic Ionomer Resin
Dow Surlyn® 1650SB
Dow Surlyn® 1706 Zinc Ionomer
Dow Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Dow Surlyn® 1601-2 Sodium Ionomer Resin for Blown and Cast Film

PDUPM101 / 33768

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.