MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene® HD-8760 LHDPE Rotational Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Rotational Molding Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8760 is fully formulated long term UV stability package in ground form.

Applications: Recreational products; Industrial components; RV tanks.

Key Words: Linear High Density Polyethylene; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.948 g/ccExxon Method
Environmental Stress Crack Resistance 8.0 hourF50, Condition B; ASTM D-1693
Melt Flow 5.0 g/10 minExxon Method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 22.0 MPaASTM D638
Elongation at Break 405 %ASTM D638
Flexural Modulus 0.930 GPaASTM D790
Impact Test 203 J
@Thickness 6.35 mm,
Temperature -40.0 °C
Impact Strength; Max Force; ARM
 
Thermal PropertiesOriginal ValueComments
Melting Point 133 °CExxon Method
Deflection Temperature at 0.46 MPa (66 psi) 57.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °CASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade
Trinseo EMERGE™ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET)
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
LyondellBasell GA675662 Petrothene® Linear Low Density Polyethylene
Bamberger Polymers Bapolene® 3039U Polyethylene, Rotational Molding Grade

PEXCFY / 37946

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.