MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Elvax® 3172Z Ethylene Vinyl Acetate  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: DuPont™ Elvax® 3172Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives: slip, antiblock.

Applications: This resin is designed to provide a low temperature heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on blown film equipment over a wide range of film thickness and blow-up ratios. It can also be coextruded with a variety of other polymers. This resin is typically used as low temperature seal layer in coextruded films.

Information provided by DuPont™

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792, ISO 1183
Vinyl Acetate Content 18 %
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 68.0 °CFreezing Point; ASTM D3417
 88.0 °CASTM D3417
Vicat Softening Point 67.0 °CASTM D1525, ISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Elvax® 3180Z Ethylene Vinyl Acetate
Dow Elvax® 3155 Ethylene Vinyl Acetate
Dow Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
Dow Elvax® 3135XZ Ethylene Vinyl Acetate
Dow Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown

PDUP921 / 33488

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.