Chemistry: Vinyl Alloy - Rigid (RPVC alloy) Description/Features: 181°F HDT, Interior, Medium Impact, High Flow Market: Electrical, Telecommunications Applications: Multi-Purpose Processing Method: Injection MoldingInformation provided by PolyOne Corporation. Geon Performance Solutions was created from PolyOne in 2019. |