MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dover Chemical 2,4 Di-Cumylphenol (DCP)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DCP is a solid at room temperature, but is typically handled as a liquid (melting point 70°). Potential applications of DCP include: antioxidant and an intermediate for low volatile benzotriazoles used as UV stabilizers.

Information provided by DoverChem

Key Words: CAS# 2772-45-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
@Temperature 70.0 °C
approximate
Molecular Weight 330 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 66.0 °Capproximate
Flash Point 330 °Capproximate
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0molten, tpyical
 <= 3.0molten
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.010 %Typical
 <= 0.050 %Spec.
 
Descriptive Properties
2,4 Dicumylphenol, %>97
 98.5typical
Appearancepale yellow liquidabove 70° C
 Pale yellow solid
Para-cumylphenol %<3
 0.3typical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER006 / 217625

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.