MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Envalior Akulon® K123, K123/A PA6, Dry, Low Viscosity
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Low Viscosity

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Water Absorption 9.5 %Sim. ISO 62
Moisture Absorption 2.50 %Humidity; Sim. ISO 62
Viscosity Number 135 cm³/gISO 307, 1157, 1628
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPaISO 527-1/-2
Elongation at Break 30 %ISO 527-1/-2
Tensile Modulus 2800 MPaISO 527-1/-2
Flexural Modulus 2700 MPaISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180/1A
Charpy Impact, Notched 7.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 150 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® F223-D PA6, Dry, Low/Medium Viscosity
Envalior Akulon® F130-E1 PA6, Medium Viscosity, Nucleated, Lubricated, Film Extrusion
DuPont Mobility and Materials Zytel® ST801 BK010A PA66-HI
Envalior Akulon® K125/A PA6
Envalior Akulon® K125 PA6

PDSM8016 / 184717

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.