MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sandvik Safeni 52 Wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Safeni 52 is a soft magnetic iron nickel alloy with high magnetic permeability, low coercive force, a low content of nonmetallic inclusions and thermal expansion properties which make it suitable for glass sealing applications. Available in strip, round wire and profile forms, Safeni 52 can be used in many applications requiring superior surface properties, accurately defined thermal expansion and high magnetic permeability. Safeni 52 is particularly suitable for glass to metal seals and has its most important application in reed switches. It is also used for thermostats in industrial applications, transistors, voltage regulators, timing devices, temperature sensitive resistors and high frequency relays.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 160Annealed
 270Cold worked
Tensile Strength, Ultimate 570 MPaAnnealed
 950 MPaCold worked
Tensile Strength, Yield 290 MPa
@Strain 0.2 %
Annealed
 910 MPa
@Strain 0.2 %
Cold worked
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000370 ohm-cm
Curie Temperature 520 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.1 µm/m-°C
@Temperature 30.0 - 500 °C
 10.2 µm/m-°C
@Temperature 30.0 - 400 °C
 10.3 µm/m-°C
@Temperature 30.0 - 300 °C
 10.4 µm/m-°C
@Temperature 30.0 - 100 °C
 10.4 µm/m-°C
@Temperature 30.0 - 200 °C
 10.8 µm/m-°C
@Temperature 30.0 - 600 °C
Specific Heat Capacity 0.460 J/g-°C
Melting Point 1435 °C
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 49 %As Balance
Nickel, Ni 51 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Safeni 48 Wire
SAE J431 heavy duty automotive gray cast iron, SAE grade G4000d
SAE J431 heavy duty automotive gray cast iron, SAE grade G3500c
Ohara S-BAL35 Optical Glass
Iron, Fe

NSANDV5057 / 199621

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.