MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer FXM1414T Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Density 1.18 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0900 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.12 %ISO 62-1
Viscosity 9.0 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cmSABIC method
 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 47.0 MPa50 mm/min; ISO 527
 48.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 56.0 MPa50 mm/min; ISO 527
 58.0 MPa50 mm/min; ASTM D638
Elongation at Break 78 %50 mm/min; ASTM D638
 89 %50 mm/min; ISO 527
Elongation at Yield 5.4 %50 mm/min; ISO 527
 5.7 %50 mm/min; ASTM D638
Tensile Modulus 2260 MPa50 mm/min; ASTM D638
 2270 MPa1 mm/min; ISO 527
Flexural Strength 85.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 88.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2120 MPa2 mm/min; ISO 178
 2230 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 520 JASTM D256
 270 J
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 57.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=1.50 mm
UL 746A
 >= 120 arcs
@Thickness >=3.00 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 67.5 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
 67.5 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
 80.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test 75.0 °CPASS; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 119 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 120 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 138 °CRate B/50; ISO 306
 139 °CRate B/50; ASTM D1525
 142 °CRate B/120; ISO 306
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
Glow Wire Ignition Temperature 825 °C
@Thickness 1.50 mm
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 800 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 310 °C
Zone 2 280 - 305 °C
Zone 3 295 - 315 °C
Melt Temperature 295 - 315 °CInjection Molding
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80293 / 288240

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.