MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Uniprene® 55A Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Features: High Elastic Recovery

Information Provided by Teknor Apex

Key Words: TPV
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 555 seconds; ASTM D2240
Tensile Strength at Break 560 psiASTM D412
Elongation at Break 300 %ASTM D412
100% Modulus 0.310 ksi
@Strain 100 %
ASTM D412
Tear Strength 16.0 kN/mDie C; ASTM D624
Compression Set 20 %
@Temperature -5.00 °C,
Time 79200 sec
Method B; ASTM D395
 27 %
@Temperature 21.1 °C,
Time 79200 sec
Method B; ASTM D395
 35 %
@Temperature 37.8 °C,
Time 79200 sec
Method B; ASTM D395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese SO.F.TER Forprene® 6NE.A75 Extrusion Grade TPE
Celanese SO.F.TER Forprene® 6NE.A65 Extrusion Grade TPE
Barlog Plastics KEBAFLEX E D 50.1 TPE-V, Shore D50
Barlog Plastics KEBAFLEX E 65.1 TPE-V, Shore A65
Barlog Plastics KEBAFLEX E 40.1 TPE-V, Shore A40

PTEKNO859 / 129040

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.