MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Honeywell Genetron® 245fa Refrigerant
Categories: Fluid

Material Notes: A non-ozone depleting candidate replacement for R-11 in centrifugal chillers. For new equipment.

Chemical Name: Pentafluoropropane

  • Chemical Notation: CF3CH2CHF2

    Information provided by Honeywell

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 82.7 lb/ft³
    @Temperature 30.0 °C
    Saturated Liquid
    Molecular Weight 134 g/mol
     
    Chemical PropertiesOriginal ValueComments
    Critical Pressure 36.4 bar
    Critical Temperature 300.29 °FASTM D1321
     
    Thermal PropertiesOriginal ValueComments
    Specific Heat Capacity 0.320 BTU/lb-°F
    @Temperature 30.0 °C
    Liquid
     0.200 BTU/lb-°F
    @Pressure 0.101 MPa,
    Temperature 30.0 °C
    Vapor
    Melting Point -160 °F
    @Pressure 0.101 MPa
    Boiling Point 58.8 °F
    @Pressure 0.101 MPa

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Geon® Performance Solutions Vinyl Flexible R245AE
    Oceanchem Group 2,4,6-Tris (2,4,6-tribromophenoxy)-1,3,5-triazine (FR245

    PHONWL117 / 179662

    Ensinger PEI

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.