MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay MIRAPOL® A-15 Surfactant
Categories: Fluid

Material Notes: Description: Cationic polymer providing good wet/dry combability properties. Imparts smooth feel, luster and detangling properties to the hair and smooth feel to the skin. Non dulling conditioning effect on fragile and fine hair. Reduces trans-epidermal water loss

C.T.F.A. /I.N.C.I. Name: POLYQUATERNIUM – 2

CAS: 68555 – 36 – 2

Recommended use level: 0.4 - 2.5 %.

Available in: Asia Pacific, Europe, Latin America and North America

Readily soluble in water in all proportions

Applications: Cationic polymer, easily dispersible in water and compatible in amphoteric surfactant systems. Highly substantive conditioning agent for skin and hair care products. Hair Care: in shampoos and hair conditioners it confers good wet-combing, dry-combing, and produces a soft natural feeling. Reduces electrostatic build-up (Flyaway). Skin Care: is highly skin substantive and provides soft feeling to the skin (liquid soaps, ...). Note: In formulating Mirapol A-15, it is necessary to dissolve the Mirapol A-15 in about 75% of the required water before addition of the remaining ingredients.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
pH 7.5 - 8.510% aq. Sol.; AN3401
Viscosity <= 3000 cP
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 34 - 38 %AN3150
 
Descriptive Properties
AppearanceClear to cloudy amber viscous liquid
Color<1000AN3013
CompositionActive62-66%, AN3150
 Chloride11-13%, AN3331
 Dichloroethylether<2 mg/kg, AN6032
 Dioxanne<5 mg/kg, AN6032
Turbidity<3.0 NTUAN3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD267 / 137498

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.