MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
International Mold Steel DHA-World Die Cast & Forging Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: DHA-World is a high hardenability and high tough general use hot work die steel.

Information provided by International Mold Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 229
Hardness, Rockwell C <= 53
Fracture Toughness 50.0 MPa-m½47 HRC
 80.0 MPa-m½43 HRC
Charpy Impact Unnotched 20.0 J/cm²49 HRC
 22.0 J/cm²47 HRC
 37.0 J/cm²44 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.3 µm/m-°C
@Temperature 20.0 - 100 °C
 12.1 µm/m-°C
@Temperature 20.0 - 300 °C
 12.8 µm/m-°C
@Temperature 20.0 - 500 °C
 13.2 µm/m-°C
@Temperature 20.0 - 700 °C
Specific Heat Capacity 0.473 J/g-°C
@Temperature 100 °C
 0.558 J/g-°C
@Temperature 300 °C
 0.667 J/g-°C
@Temperature 500 °C
 0.934 J/g-°C
@Temperature 700 °C
Thermal Conductivity 25.2 W/m-K
@Temperature 100 °C
 27.6 W/m-K
@Temperature 700 °C
 27.9 W/m-K
@Temperature 300 °C
 28.7 W/m-K
@Temperature 500 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
International Mold Steel DH31-EX Die Cast & Forging Steel
International Mold Steel DH21 Die Cast & Forging Steel
EDRO #7 Shock Resistant S7 Tool Steel
Carpenter S7 Alloy Tool Steel (AISI S7)
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel

NIMSA09 / 175989

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.