MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® PLUS PLS95G35DH1 BK031 Nylon  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptional resistance in hot air & hot engine oil.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccDAM; ISO 1183
Filler Content 35 %DAM
Moisture Absorption at Equilibrium 1.8 %
@Temperature 23.0 °C
50% RH; from DAM; ISO 62, Similar to
Water Absorption at Saturation 6.0 %
@Temperature 23.0 °C
By immersion; ISO 62, Similar to
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0075 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 135 MPa
@Temperature 23.0 °C
50%RH; ISO 527
 210 MPa
@Temperature 23.0 °C
DAM; ISO 527
Elongation at Break 3.5 %
@Temperature 23.0 °C
DAM; ISO 527
 7.0 %
@Temperature 23.0 °C
50%RH; ISO 527
Tensile Modulus 7500 MPa
@Temperature 23.0 °C
50%RH; ISO 527
 11000 MPa
@Temperature 23.0 °C
DAM; ISO 527
Flexural Strength 316 MPa
@Temperature 23.0 °C
DAM; ISO 178
Flexural Modulus 9800 MPa
@Temperature 23.0 °C
DAM; ISO 178
Charpy Impact Unnotched 68.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 70.0 kJ/m²
@Temperature -30.0 °C
50%RH; ISO 179/1eU
 87.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
50%RH; ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.70e+14 ohm-cm
@Temperature 23.0 °C
50%RH; IEC 60093
 7.00e+14 ohm-cm
@Temperature 23.0 °C
50%RH; ASTM D257
 3.00e+16 ohm-cm
@Temperature 23.0 °C
DAM; ASTM D257
 3.00e+16 ohm-cm
@Temperature 23.0 °C
DAM; IEC 60093
Surface Resistance 4.50e+14 ohm
@Temperature 23.0 °C
50%RH; IEC 60093
 5.00e+14 ohm
@Temperature 23.0 °C
50%RH; ASTM D257
 1.00e+15 ohm
@Temperature 23.0 °C
DAM; ASTM D257
 1.00e+15 ohm
@Temperature 23.0 °C
DAM; IEC 60093
Comparative Tracking Index >= 600 V
@Temperature 23.0 °C
DAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 12.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
DAM; ISO 11359-1/-2
Melting Point 266 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 263 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °CDAM; ISO 75-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °CDAM
 290 °CDAM; Optimum
Mold Temperature 70.0 - 120 °CDAM
 100 °CDAM; optimum
Drying Temperature 80.0 °CDAM
Dry Time 2.00 - 4.00 hourDAM
Moisture Content <= 0.20 %DAM
 
Descriptive Properties
AppearanceBlack ColorDAM
Drying RecommendedYes, if moisture content of resin exceeds recommended levelDAM
FeaturesCopolymerDAM
 Flow, GoodDAM
 Thermal Stability, GoodDAM
FillerGlass ReinforcedDAM
FormsPelletsDAM
GenericNylon 6DAM
Material StatusPreliminary DataDAM
Part Marking Code>PA-GF35<ISO 11469; DAM
Polymer FamilyPolyamideDAM
Polymer TypePADAM
Processing MethodInjection MoldingDAM
Product CategoryGlass Reinforced ResinsDAM
 SHIELD Technology ResinsDAM
Region Available - GlobalYesDAM
Resin IdentificationPA-GF35ISO 1043; DAM
Ultrasonic WeldableYesDAM
UsesAutomotive ApplicationsDAM
 Automotive Under the HoodDAM
 High Temperature ApplicationsDAM

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 103FHSA NC010 PA66
Celanese Zytel® 151L NC010 PA612
Celanese Elvamide® 8061 PA6/66/610
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
Celanese Zytel® 77G33HS1L NC010 Nylon 612

PZDSZ1461 / 140278

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.