Co-extruded PC/PC+ABS Sheet ALLEN® Alextra™ MV has an excellent weatherable performance and property retention. It has the most versatile (MV) and best economics in the product line. ALLEN® Alextra™ MV is Underwriters Laboratories, Inc® recognized for UL Std 94 HB (UL94) Suggested Applications: - Industrial
- Heavy Truck
- Recreational Vehicles
- Personal Recreation
- Auto After-Market
- Agriculture / Construction
Features: - Excellent physical property retention
- Good low temperature impact
- High heat deflection temperature
- Improved performance over ABS
- Higher modulus (Increased stiffness)
Information provided by Sekisui Polymer Innovations |