MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sinotek Materials Graphite Sealing Strip Fireproofing Sealing Products
Categories: Carbon; Graphite

Material Notes: The graphite sealing strip is made from a graphite based mineral fiber with stabilized high density, which is designed to activate (expand) at 180° with an expansion ratio of 35:1. The intumescent strip around the door expands at high temperatures to seal housing and provide a ‘flame break’. It can adhibit on windowsills, door-apertures, and all kinds of pipe-line apertures, etc. When fire or high temperature occurs, and expand temperature is achieved, it can expand and block the aperture completely. This materials usually is used on buildings.

Information provided by Sinotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Expansion Ratio, %3500

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Graphite, Carbon, C
NeoGraf eGRAF® HITHERM™ HT-710 Graphite
NeoGraf GRAFCELL® FFP-300 SERIES Flow Field Plate Graphite
Pyrolytic Graphite, Low Temperature Isotropic (LTI)
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating

CSINOT84 / 2141

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.