Physical Properties | Original Value | Comments |
---|
Density | 1.79 g/cc |
Moisture Absorption | 1.20 % |
Linear Mold Shrinkage, Flow | 0.0040 cm/cm |
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm |
|
Mechanical Properties | Original Value | Comments |
---|
Tensile Strength at Break | 65.0 MPa @Temperature 200 °C |
| 75.0 MPa @Temperature 180 °C |
| 80.0 MPa @Temperature 120 °C |
| 95.0 MPa @Temperature 160 °C |
| 100 MPa @Temperature 100 °C |
| 115 MPa @Temperature 150 °C |
| 140 MPa @Temperature 80.0 °C |
| 180 MPa @Temperature 120 °C |
| 210 MPa @Temperature 100 °C |
| 230 MPa @Temperature 40.0 °C |
| 230 MPa @Temperature 80.0 °C |
| 250 MPa @Temperature 23.0 °C |
| 260 MPa @Temperature 40.0 °C |
| 270 MPa @Temperature 23.0 °C |
| 320 MPa @Temperature -40.0 °C |
| 330 MPa @Temperature -40.0 °C |
Elongation at Break | 1.65 % @Temperature 40.0 °C |
| 1.75 % @Temperature -40.0 °C |
| 1.75 % @Temperature 40.0 °C |
| 1.8 % @Temperature 23.0 °C |
| 1.8 % @Temperature -40.0 °C |
| 1.8 % @Temperature 80.0 °C |
| 1.8 % @Temperature 100 °C |
| 1.85 % @Temperature 23.0 °C |
| 1.9 % @Temperature 120 °C |
| 2.6 % @Temperature 80.0 °C |
| 3.0 % @Temperature 100 °C |
| 3.3 % @Temperature 120 °C |
| 3.5 % @Temperature 150 °C |
| 4.0 % @Temperature 160 °C |
| 4.0 % @Temperature 180 °C |
| 4.0 % @Temperature 200 °C |
Tensile Modulus | 7400 MPa @Temperature 200 °C |
| 8100 MPa @Temperature 180 °C |
| 9500 MPa @Temperature 120 °C |
| 9800 MPa @Temperature 160 °C |
| 10900 MPa @Temperature 100 °C |
| 12500 MPa @Temperature 150 °C |
| 17800 MPa @Temperature 80.0 °C |
| 20500 MPa @Temperature 120 °C |
| 21500 MPa @Temperature 100 °C |
| 22000 MPa @Temperature 80.0 °C |
| 22500 MPa @Temperature 40.0 °C |
| 23000 MPa @Temperature 23.0 °C |
| 23500 MPa @Temperature 40.0 °C |
| 23800 MPa @Temperature 23.0 °C |
| 24000 MPa @Temperature -40.0 °C |
| 25000 MPa @Temperature -40.0 °C |
Flexural Strength | 390 MPa |
| 420 MPa |
Flexural Modulus | 2400 MPa @Temperature 23.0 °C |
| 8200 MPa @Temperature 200 °C |
| 9000 MPa @Temperature 180 °C |
| 12000 MPa @Temperature 160 °C |
| 20000 MPa @Temperature 120 °C |
| 23500 MPa @Temperature 23.0 °C |
Charpy Impact Unnotched | 75.0 kJ/m² @Temperature 23.0 °C |
| 75.0 kJ/m² @Temperature -30.0 °C |
| 75.0 kJ/m² @Temperature -30.0 °C |
| 90.0 kJ/m² @Temperature 23.0 °C |
Charpy Impact, Notched | 11.0 kJ/m² @Temperature 23.0 °C |
| 12.0 kJ/m² @Temperature -30.0 °C |
| 13.0 kJ/m² @Temperature 23.0 °C |
| 13.0 kJ/m² @Temperature -30.0 °C |
|
Electrical Properties | Original Value | Comments |
---|
Dielectric Strength | 19.0 kV/mm |
| 19.0 kV/mm |
Comparative Tracking Index | 425 V |
|
Thermal Properties | Original Value | Comments |
---|
CTE, linear | 41.0 µm/m-°C |
CTE, linear, Parallel to Flow | 13.0 µm/m-°C |
Melting Point | 330 °C |
Maximum Service Temperature, Air | 176 °C |
Deflection Temperature at 1.8 MPa (264 psi) | 307 °C |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to go back to viewing the property data in MatWeb's normal format.