MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Superior Flux Superior No. 465 High Activity, Zinc-Free Brass Tinning Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Continuous Brass Tinning Flux for Copper and Brass Strip

    Excellent Rapid Oxide Removal Properties

  • Zinc-Free and Ammonia-Free Formulation
  • Can be Used for Tinning of Steel Wire and Hard-to-Solder Copper Alloys
  • Does Complete Tinning of Strip or Wire Surfaces with a Single Pass
  • Completely Water-based Formulation, No Solvents and No Alcohols
Description: Superior No. 465 is a zinc-free, metal halide / organic base - inorganic acid type flux. The fluxing ingredients of Superior No. 465 flux offers a high degree of fluxing activity in the soldering and tinning temperature ranges for continuous brass strip and steel wire tinning. Superior No. 465 leaves minimal, zinc-free residue in the tinning pot as the strip or wire is submerged during tinning.

Applications: Superior No. 465 was formulated for continuous hot dip tinning of copper and brass strip. This formulation, fully concentrated, will also work for steel wire tinning. Normal flux application such as total immersion of the brass strip or steel wire in flux is recommended. Non-continuous applications will work by adding flux by part immersion or by brush.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 - 1.15 g/cc
Density 9.50 lb/gal
Surface Tension 32 dynes/cm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 427 °CSoldering Range
Shelf Life 2.00 Month
 
Descriptive Properties
AppearanceClear, Colorless to Yellow
Free Acid11.5-15.5%HCl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSFLUX069 / 185753

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.