MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® MonoPlus M 880 KR Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus M 880 KR is a strongly basic, gel type anion exchange resin (type I) with a monodisperse distribution of particle size based on a styrene-divinylbenzene copolymer. Lewatit MonoPlus M 880 KR is manufactured in its high-regenerated form (minimum 95% of OH). Lewatit nuclear resins (Lewatit KR) are highly purified resins which have got a very good stability to mechanical and chemical influence, and to osmotic shocks as well. They allow high velocities due to their excellent hydrodynamic properties. As their monodispersity is very high (uniformity coefficient max. 1.1) and their content of fines very low (max 0.1% for beads <0.315 mm) lower losses of pressure can be achieved compared with standard resins. If they are used in water circuits contaminated with radioactive material, they safeguard a water quality with fully matches the highest demands of the nuclear power industry. Lewatit MonoPlus M 880 KR is specially suited for:
  • the removal of arsenic including radioactive isotopes from aqueous solutions (including boric acid)
  • decontamination of cooling water circuits in nuclear power plants
  • the use in primary cooling circuits of boiling water and pressurized water reactors
  • cleaning in the blow down process independent on the conditioning with corrosion inhibitors (either hydrazine, morpholine or ethanolamine)
  • polishing both in the primary and secondary circuits as a component in mixed beds, combined with Lewatit MonoPlus SP 112 KR or Lewatit MonoPlus S 200 KR.
IMPORTANT! If the Lewatit MonoPlus M 880 KR mixed with Lewatit MonoPlus SP 112 KR or Lewatit MonoPlus S 200 KR, the Lewatit MonoPlus M 880 KR must be thoroughly washed out with demineralized water.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.680 g/cc
Density 1.07 g/cc
Bead Size 0.590 - 0.690 mmMean
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceAmber, translucent
pH Operating Range0 - 12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8784 / 209176

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.