MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nilit Polynil® P230 High Viscosity Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Description: Polynil P230 is a high viscosity NYLON 66 (Viscosity number 280 cm³/gr) that was developed for film- and rod extrusion. It has high melt stability and low gel content. It holds various food approvals.

Key characteristics:

  • Viscosity number 280 cm3/gr
  • Low gel content
  • Various food contact approvals
  • High heat stability

Information provided by NILIT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Viscosity Measurement 230relative viscosity (formic acid); ASTM D789
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 11900 psiASTM D638
Elongation at Break 142 %ASTM D638
Tensile Modulus 393000 psiASTM D638
Flexural Strength 17250 psiASTM D790
Flexural Modulus 408 ksiASTM D790
Izod Impact, Notched (ISO) 3.30 ft-lb/in²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 450 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 158 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity
Envalior Akulon® K222-DL PA6, Conditioned, Low Viscosity, Heat Stabilized, Light Stabilized
Envalior Akulon® K222-D PA6, Dry, Low Viscosity
Envalior Akulon® K222-D PA6, Conditioned, Low Viscosity
Envalior Akulon® K222-D (Cond.) Low Viscosity Nylon 6 (North America)

PLBN19 / 50408

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.