MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Delo® Extended Life Coolant System, Coolant/Antifreeze
Categories: Fluid

Material Notes: Features

Delo Extended Life Coolant/Antifreeze products are heavy duty engine coolants that use a patented organic corrosion inhibitor technology called carboxylates. The product line consists of Delo Extended Life Coolant/Anti-Freeze Concentrate, Delo Extended Life Prediluted 50/50 Coolant/Anti-Freeze and Delo Extender.

Delo Extended Life Coolant/Antifreezeconcentrate is ethylene glycol based and contains Chevron`s patented carboxylate technology. This product does not contain conventional inhibitors like silicates, nitrates, amines, phosphates or borates. Delo ELC concentrate can be used for initial fill or top up but it must diluted. It should be used full strength for freeze point adjustment.

Delo Extended Life Prediluted 50/50 Coolant/Antifreeze is a 50/50 mixture of Delo Extended Life Coolant/Antifreeze concentrate with deionized water for freeze protection down to -37°C and boil over protection to 129°C with a 15 lb pressure cap. Delo ELC Prediluted 50/50 is recommended for top up and can be used for initial fill.

Delo Extender should be added to Delo ELC at 500,000 miles/10,000 hours/4 years to reach a coolant service life of 1,000,000 miles/20,000 hours/8 years. The amount of Extender needed is based on the volume of the cooling system. Extender should only be added once during the service life of Delo ELC.

Applications

The patented carboxylate technology in Delo ELC can be used in on-road, off-road and stationary engine applications. Delo ELC protects all cooling system components and has proven over years of field testing and customer use to improve water pump life and improve heat transfer. The inhibitors in Delo ELC do not readily deplete and for this reason there is no need to add SCAs or test the coolant/antifreeze as is required when using conventional coolants requiring SCA additions.

In service Delo ELC is recommended for use out to 750,000 miles/15,000 hours/8 years. If even longer service intervals are desired then the addition of Delo Extender at 500,000 miles/10,000 hours/4 years will extend the service life to 1,000,000 miles/20,000 hours/8 years.

When using Delo ELC it is not recommended that supplemental coolant additives be used. If an accidental addition of SCAs should happen it will not create any operational issues. Additions of SCAs to Delo ELC increases the overall cost of maintenance and adds inhibitors that are not needed for ELC to perform at maximum levels of protection. Delo ELC products are dilution tolerant up to 25% percent with other non-Delo ELC products or water. Dilution of more then 25% will reduce the extended life properties of this product. When using Delo ELC it is recommended that the product freeze point be maintained between -12°F and -62°F. If the freeze point is higher or lower than the range specified it is an indication that water or concentrated coolant has been added to the system. To adjust freeze point for over or under concentration use the tables at the end of this document.

Note: These products are not to be used to protect the inside of potable water systems against freezing.

Key Words: CPS Number: 227804; MSDS Number: 10391
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/cc
pH 8.31:2 dilution with water; ASTM D1287
 
Thermal PropertiesOriginal ValueComments
Melting Point -37.0 °C
 
Descriptive Properties
ColorRed
Reserve Alkalinity ASTM D11216
Silicate, %None

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco SUPREME Antifreeze/Coolant, Concentrate
ChevronTexaco HDAX® 50/50 Coolant
ChevronTexaco DEX-COOL® Extended Life Antifreeze/Coolant, Prediluted 50/50
ChevronTexaco DEX-COOL® Extended Life Antifreeze/Coolant, Concentrate
ExxonMobil Coolant/Antifreeze Mobil Heavy Duty

WCHEV415 / 75030

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.