WESTLAKE HIFOR Polyethylene LT74155 is a high strength linear low density polyethylene containing no slip, high antiblock and processing aid. It is designed for blown film applications and is well suited for consumer and industrial packaging markets which require impact and tear strength. Films produced using LT74155 exhibit low imperfections and facilitate production at thinner gauges.Application/Uses- Vegetable packaging
- Bread bags
- Ice bags
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical |