MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
BASF 3D Ultrafuse® PP Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Components: Polypropylene based filament for Fused Filament Fabrication.

Product Description: Ultrafuse PP is high-performance thermoplastic with low density, high elasticity and high resistance to fatigue. The mechanical properties make it an ideal material for 3D-printing applications which have to endure high stress or strain. The filament has high chemical resistance and a high isolation value. PP is one of the most used materials in the world, due to its versatility and ability to engineer lightweight tough parts.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.911 g/ccPrinted Part; ISO 1183-1
Melt Flow 6.1037 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 9.00 MPaZX: Upright; ISO 527
 15.5 MPaXY: Flat; ISO 527
Elongation at Break 5.4 %ZX: Upright; ISO 527
 118.6 %XY: Flat; ISO 527
Modulus of Elasticity 0.435 GPaYoung's, ZX: Upright; ISO 527
 0.541 GPaYoung's, XY: Flat; ISO 527
Flexural Strength 15.6 MPaZX: Upright; ISO 178
 21.4 MPaXZ: On its edge; ISO 178
 22.9 MPaXY: Flat; ISO 178
Flexural Modulus 380 MPaZX: Upright; ISO 178
 494 MPaXZ: On its edge; ISO 178
 575 MPaXY: Flat; ISO 178
Flexural Strain at Break 7.9 %ZX: Upright; ISO 178
 8.8 %XZ: On its edge; ISO 178
 9.4 %XY: Flat; ISO 178
Izod Impact, Notched (ISO) 2.30 kJ/m²ZX: Upright; ISO 180
 5.30 kJ/m²XY: Flat; ISO 180
 10.6 kJ/m²XZ: On its edge; ISO 180
Izod Impact, Unnotched (ISO) 11.6 kJ/m²ZX: Upright; ISO 180
 37.6 kJ/m²XZ: On its edge; ISO 180
 37.7 kJ/m²XY: Flat; ISO 180
Charpy Impact Unnotched 13.6 kJ/m²ZX: Upright; ISO 179-2
 41.8 kJ/m²XY: Flat; ISO 179-2
 62.3 kJ/m²XZ: On its edge; ISO 179-2
Charpy Impact, Notched 2.50 kJ/m²ZX: Upright; ISO 179-2
 5.30 kJ/m²XY: Flat; ISO 179-2
 8.30 kJ/m²XZ: On its edge; ISO 179-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 131 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 54.0 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °CISO 75-2
Glass Transition Temp, Tg 83.0 °CISO 11357-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CBed, Bed Material: PP tape or PP adhesive
Nozzle Temperature 220 - 240 °C
Drying Temperature 60.0 °Cin a hot air dryer or vacuum oven
Dry Time 4.00 - 16.0 hour
Shelf Life 12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.4 mm
Print speed20-50 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASF3D004 / 312245

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.