Metallocene medium density polyethylene. This metallocene MDPE resin is tailored for blow molded containers that require: - High gloss
- Good clarity
- Excellent ESCR
Applications: Typical blow molded applications for C300 include: - Glossy multilayer bottles
- Squeezable bottles
Information provided by Phillips This resin meets these specifications: - ASTM D4976 - PE 224
- FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)
|