MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Chi Mei Polyrex® PH-55Y Polystyrene Resin
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: For general injection/for injection blowing. Medium Impact. Applications: General injection including injection blowing for food containers, beverage containers, toy casings, piano keyboards and parts.

POLYREX® PS resin is a solid polymer formed by heat polymerization of styrene (SM). High Impact Polystyrene (HIPS) composed of SM and butadiene (BD). HIPS is high impact resistant and non-transparent. POLYREX® is suitable for home appliances, food and water contact materials, toys, and construction materials, and especially appliance housings due to its excellent processability.

Information provided by Chi Mei Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmISO 294-4
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 220 °C
Melt Volume Rate (ml/10 min.); ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25.0 MPa50 mmm/min; ISO 527
Tensile Strength, Yield 27.0 MPa50 mm/min; ISO 527
Elongation at Break 60 %50 mm/min.; ISO 527
Flexural Strength 38.0 MPa2 mm/min.; ISO 178
Flexural Modulus 1.30 GPa2 mm/min.; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
@Temperature -30.0 °C
180/1A
 7.00 kJ/m²
@Temperature 23.0 °C
180/1A
Charpy Impact, Notched 3.60 kJ/m²
@Temperature -30.0 °C
ISO 179
 6.00 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 - 60.0 µm/m-°CISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °Cannealed; ISO 75A
 87.0 °Cannealed; ISO 75A
Vicat Softening Point 87.0 °C
@Load 5.00 kg
50°C/hr; ISO 306
 94.0 °C
@Load 1.00 kg
50°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHI9905 / 280798

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.