Austenitic stainless steel for high temperatures, ASTM TP347, 347H Sandvik 8R40 is an austenitic, niobium-stabilized stainless chromium-nickel steel for use at temperatures up to 850°C (1560°F). Information provided by Sandvik ASTM 347; UNS S34700; EN 1.4550 |