MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® CP-32263 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-32263 is a high performance thermoplastic elastomer, available in NAT and colors, designed for a variety of consumer product applications, including seals and gaskets, requiring low extraction by various solvent. Monprene CP-32263 is a high clarity, medium hardness, low density, elastic grade with good flow that is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Processability; High Clarity; Kink Resistant; Low Density; Low Extractables; Low Specific Gravity; Medium Hardness; Resilient; Solvent Resistant

Uses: Gaskets; Insulation; O-rings; Rubber Replacement; Seals; Tubing; Washer

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 64
@Time 5.00 sec
ASTM D2240
 67
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 1720 psiASTM D412
Tensile Stress at Strain 325 psi
@Strain 50 %
ASTM D412
 385 psi
@Strain 100 %
ASTM D412
 615 psi
@Strain 300 %
ASTM D412
Elongation at Break 630 %ASTM D412
Tear Strength 247 pliASTM D624
Compression Set 18 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 86 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Processing Temperature 380 - 440 °FMelt, Injection
Rear Barrel Temperature 300 - 340 °FInjection
Middle Barrel Temperature 340 - 380 °FInjection
Front Barrel Temperature 380 - 440 °FInjection
Nozzle Temperature 380 - 440 °FInjection
Zone 1 340 - 370 °FExtrusion
Zone 2 360 - 385 °FExtrusion
Zone 3 365 - 400 °FExtrusion
Zone 4 400 - 440 °FExtrusion
Zone 5 400 - 440 °FExtrusion
Die Temperature 400 - 440 °FExtrusion
Mold Temperature 70.0 - 125 °FInjection
Back Pressure 50.0 - 150 psiInjection
Cushion 0.140 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0831 / 237322

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.