Physical Properties | Original Value | Comments |
---|
Volatiles | <= 1.5 % @Temperature 135 °C |
Thickness | 9.00 mil |
|
Mechanical Properties | Original Value | Comments |
---|
Tensile Strength, Yield | 549 - 693 psi |
| 840 psi |
| 47000 psi @Temperature 93.3 °C |
| 52000 psi @Temperature 71.1 °C |
| 59000 psi @Temperature 21.1 °C |
| 65000 psi @Temperature 71.1 °C |
| 72000 psi @Temperature 21.1 °C |
| 95000 psi @Temperature -53.9 °C |
Tensile Modulus | 3300 ksi @Temperature 71.1 °C |
| 3400 ksi @Temperature 21.1 °C |
| 3500 ksi @Temperature -53.9 °C |
| 3700 ksi @Temperature 21.1 °C |
| 3700 ksi @Temperature 71.1 °C |
| 3900 ksi @Temperature 93.3 °C |
Flexural Strength | 65.0 ksi @Temperature 71.1 °C |
| 66.0 ksi @Temperature 93.3 °C |
| 77.0 ksi @Temperature 71.1 °C |
| 80.0 ksi @Temperature 21.1 °C |
| 95.0 ksi @Temperature 21.1 °C |
| 117 ksi @Temperature -53.9 °C |
Flexural Modulus | 2700 ksi @Temperature 71.1 °C |
| 2800 ksi @Temperature 93.3 °C |
| 2900 ksi @Temperature 71.1 °C |
| 3000 ksi @Temperature 21.1 °C |
| 3200 ksi @Temperature -53.9 °C |
| 3200 ksi @Temperature 21.1 °C |
Compressive Strength | 47.0 ksi @Temperature 71.1 °C |
| 52.0 ksi @Temperature 93.3 °C |
| 55.0 ksi @Temperature 71.1 °C |
| 56.0 ksi @Temperature 21.1 °C |
| 66.0 ksi @Temperature 21.1 °C |
| 84.0 ksi @Temperature -53.9 °C |
Compressive Modulus | 3500 ksi @Temperature 71.1 °C |
| 3500 ksi @Temperature 71.1 °C |
| 3500 ksi @Temperature 93.3 °C |
| 3600 ksi @Temperature 21.1 °C |
| 3600 ksi @Temperature 21.1 °C |
| 3700 ksi @Temperature -53.9 °C |
Shear Strength | 5.20 ksi @Temperature 93.3 °C |
| 6.00 ksi @Temperature 71.1 °C |
| 6.50 ksi @Temperature 71.1 °C |
| 8.00 ksi @Temperature 21.1 °C |
| 9.00 ksi @Temperature 21.1 °C |
| 11.5 ksi @Temperature -53.9 °C |
|
Electrical Properties | Original Value | Comments |
---|
Dielectric Constant | 4.2 @Frequency 9.375e+9 Hz |
| 4.2 @Frequency 1.80e+10 Hz |
Dissipation Factor | 0.013 @Frequency 9.375e+9 Hz |
| 0.013 @Frequency 1.80e+10 Hz |
|
Thermal Properties | Original Value | Comments |
---|
Glass Transition Temp, Tg | 115 °C |
|
Processing Properties | Original Value | Comments |
---|
Gel Time | 4.00 min |
Shelf Life | 12.0 Month @Temperature -17.8 °C |
|
Descriptive Properties |
---|
Climbing Drum Peel (in-lb/3in) | 14.7 |
| 14.8 |
Fabric Area Weight (g/m²) | 303.5 |
Long Beam Flexure (P/Y lb/in) | 152 / 124 |
| 201 |
Long Beam Flexure Strength (lbs) | 157 / 130 |
| 205 |
Prepreg Resin Content (%) | 39 |
Resin Flow (%) | 14 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to go back to viewing the property data in MatWeb's normal format.