MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Soluble D
Categories: Fluid; Lubricant

Material Notes: Texaco Soluble Oil D delivers value through:
  • No separation — Excellent emulsion even with hard water
  • Rust protection for steel work and machined parts even when water-oil emulsion ratios are eighty to one
  • Ability to control bacterial growth and rancid odors
  • Cooling improved by metal wetting. Also good chip settling.
  • Reduced foaming — Possibility of sump overflow minimized.
  • Stability in storage — Will not turn rancid.

Texaco Soluble Oil D is an emulsifying oil which readily mixes with water, forming a homogeneous and exceptionally stable emulsion. It provides rust and corrosion inhibition and foam inhibition. It is used in the machining of both ferrous and nonferrous metals, particularly when cutting with carbon or high speed steel or tungsten carbide tools. It also combats bacterial growth in machine sumps.

Texaco Soluble Oil D is used broadly in machine shop operations as a multifunctional cutting fluid. It is designed primarily to cool and lubricate the contact point of the tool and the work piece. It also prevents rusting or corrosion of the metals being machined as well as controls growth of bacteria, which is a constant problem in soluble oil circulating systems due to outside contamination.

Texaco Soluble Oil D minimizes surface foam and speeds the release of entrained air which could cause pump cavitation. This is a versatile fluid designed to meet many of the situations encountered in the metalworking industry.

Texaco Soluble Oil D is recommended for all metals (except magnesium) where maximum cooling is desired, particularly when cutting with carbon, high speed steel, or tungsten carbide tools.

Texaco Soluble Oil D is used extensively in milling, drilling, gear cutting, turning, planing, shaping, sawing, and grinding operations.

One gallon of Texaco Soluble Oil D for each 20 gallons of water satisfies most cutting operations; however, the add oil to water to avoid forming sticky invert emulsions which do not emulsify properly in water. See the Soluble Oil Mixing Recommendations chart for the proper ratio for the application.

Texaco Soluble Oil D is suitable for use in automotive cooling systems to prevent rust and corrosion. A mixture of forty to one is most often used. However, always follow engine manufacturers recommendations. It is preferable to mix radiator water and oil in a separate container. Additions to the radiator should be made from this container. As with any other "additives", the radiator should be drained and flushed occasionally, since evaporation and leakage cause proportions to change.

Do not recommend Texaco Soluble Oil D emulsions for magnesium. Hot magnesium is a fire hazard when it contacts water. The preferred recommendation is Texaco Alcaid® 19 (ISO 22).

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 220786; MSDS Number: 8625

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 20.4 °
Saybolt Viscosity at 100°F 198 SUS
Saybolt Viscosity at 210°F 43.7 SUS
Kinematic Viscosity at 40°C (104°F) 38 cSt
Kinematic Viscosity at 100°C (212°F) 5.2 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -30.0 °C
Flash Point 160 °C
 
Component Elements PropertiesOriginal ValueComments
Sulfur, S 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Transultex® H

WTEXA292 / 77171

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.