MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Phillips 66 Type A ATF
Categories: Fluid; Lubricant

Material Notes: Type F ATF is specifically designed for use in automatic transmissions in passenger cars and light trucks manufactured by Ford Motor Company prior to 1977, and in many 1977-1981 models. It also is recommended for use in many Borg-Warner automatic transmissions and older Ford power steering units, as well as in the hydrostatic drive systems and hydraulic systems on certain farm equipment. Type F ATF is formulated to provide the proper frictional characteristics for positive shifting with little or no slippage. It has excellent oxidation resistance and thermal stability at high temperatures to minimize sludge and varnish formation, and provide long service life. It provides good wear protection, protects against rust and corrosion, and has good foam resistance. It also has good low-temperature properties for easier shifting in cold weather.

Applications:

  • Service fill in all automatic transmissions and power steering units that require a fluid meeting the requirements of Ford specification ESW-M2C33-F
  • Hydrostatic drive systems and hydraulic systems on certain farm equipment
Type F ATF is not recommended for use in transmissions that require any other type of automatic transmission fluid besides Type F. Type F ATF meets or exceeds the requirements of:
  • Ford ESW-M2C33-F (obsolete specification)
QPL Approval Numbers: D07L1-50 (Type A 100AD), D07L1-60 (Type A 120AD)

Features/Benefits:

  • Proper frictional properties for transmissions that require a fluid with high static friction
  • Excellent oxidation resistance and thermal stability
  • Protects against sludge and varnish formation
  • Protects against wear
  • Protects against rust and corrosion
  • Good low-temperature properties
  • Good seal compatibility
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.864 g/cc
Density 7.20 lb/gal
Brookfield Viscosity 1100 cP
@Temperature -18.0 °C
Viscosity Measurement 146Index
Kinematic Viscosity at 40°C (104°F) 43 cSt
Kinematic Viscosity at 100°C (212°F) 7.6 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point <= -40.0 °C
Flash Point 210 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn 0.048 %
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON6333 / 210099

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.