LL0220KJ is linear low density polyethylene copolymer containing butene-1(C4) as comonomer. It is suitable for blending with conventional. LDPE for blown film applications. Film made from pure LL0220KJ has the following advantages over LDPE: good balance of mechanical properties, good optical properties, easy opening properties in 2 layer film. This grade has food contact approval. Applications: light and medium duty films with good optical properties.Information provided by Tabriz Petrochemical Company. |