MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ovako 24MnV6* SB600 Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: Grade SB600 is a micro-alloyed steel for general purposes. It is recommended for applications requiring high yield strength in the as rolled condition. The chemical composition has no standardized equivalent, but is unique to Ovako Bar.

Information provided by Ovako

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 210 - 265
@Thickness 15.0 - 30.0 mm
Flat bar
 210 - 265
@Thickness 30.0 - 60.0 mm
Flat bar
 215 - 265
@Thickness 30.0 - 80.0 mm
Round bar
 225 - 265
@Thickness 15.0 - 30.0 mm
Round bar
 215 - 280
@Thickness 5.00 - 15.0 mm
Flat bar
 240 - 280
@Thickness <=15.0 mm
Round bar
Tensile Strength 700 - 870 MPa
@Thickness 15.0 - 30.0 mm
Flat bar
 700 - 870 MPa
@Thickness 30.0 - 60.0 mm
Flat bar
 740 - 870 MPa
@Thickness 30.0 - 80.0 mm
Round bar
 780 - 870 MPa
@Thickness 15.0 - 30.0 mm
Round bar
 740 - 920 MPa
@Thickness 5.00 - 15.0 mm
Flat bar
 820 - 920 MPa
@Thickness <=15.0 mm
Round bar
Tensile Strength, Yield >= 540 MPa
@Thickness 30.0 - 60.0 mm
Reh, Flat bar
 >= 570 MPa
@Thickness 15.0 - 30.0 mm
Reh, Flat bar
 >= 570 MPa
@Thickness 30.0 - 80.0 mm
Reh, Round bar
 >= 600 MPa
@Thickness 5.00 - 15.0 mm
Reh, Flat bar
 >= 600 MPa
@Thickness <=15.0 mm
Reh, Round bar
 >= 600 MPa
@Thickness 15.0 - 30.0 mm
Reh, Round bar
Elongation at Break 14 %
@Thickness <=15.0 mm
Round bar
 14 %
@Thickness 15.0 - 30.0 mm
Round bar
 14 %
@Thickness 30.0 - 80.0 mm
Round bar
 14 %
@Thickness 5.00 - 15.0 mm
Flat bar
 14 %
@Thickness 15.0 - 30.0 mm
Flat bar
 14 %
@Thickness 30.0 - 60.0 mm
Flat bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 407 °CMS
 721 °CAC1
 820 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.20 - 0.25 %
Iron, Fe 97.3 - 99.05 %As Balance
Manganese, Mn 0.60 - 1.65 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.15 - 0.54 %
Sulfur, S <= 0.035 %
Vanadium, V <= 0.20 %
 
Descriptive Properties
WeldabilityCEV 0.47max
 Pcm 0.32max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NOVAKO191 / 234490

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.