MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Herculoy®, High-Silicon Bronze A, UNS C65500, OS035 Temper, Flat Products & Wire
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: Nominal Grain Size 0.035 mm

Fabrication Properties: Excellent Suitability – Brazing, Gas Shielded Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Soldering, Oxyacetylene Welding; Fair Suitability – Coated Metal Arc Welding

Common Fabrication Processes: Blanking; Drawing; Forming and Bending; Heading and Upsetting; Hot Forging and Pressing; Roll Threading and Knurling; Shearing; Squeezing and Swaging

Typical uses: Sculpture; Motors, Rotor Bar; Pole Line Hardware; Bolts; Clamps; Cotter Pins; Hinges; Nails; Rivets; Screws; Bearing Plates; Bushings; Butts; Cable; Channels; Chemical Equipment; Doctor Blades, Paper Industry; Heat Exchanger Tubes; Hydraulic Pressure Lines; Kettles; Oil Refinery Plumbing Tube; Piston Rings; Pressure Vessels; Screen Cloth; Screen Plates; Shafting; Tanks; Wear Plates; Welded Pressure Vessels; Welded Tanks; Wire; Hardware; Propeller Shafts

Applicable Specifications: Bar – B124/B124M, SAE J461, SAE J463; Bolts – ASTM F468; Forgings, Die (Hot Pressed) – ASME SB283, ASTM B283/B283M; Nuts – ASTM F467; Plate - Bridge and Bearing ASTM B100; Rod – SAE J463, Forgings ASTM B124/B124M, SAE J461; Rod, Bar & Shapes - Copper-Silicon Alloy ASTM B98/B98M, Copper-Silicon Alloy ASME SB98; Screws – ASTM F468; Seamless Pipe and Tube – ASTM B315, ASME SB315; Shapes – SAE J463, Forgings ASTM B124/B124M, SAE J461; Sheet – SAE J461, SAE J463, Bridge and Bearing ASTM B100; Sheet, Strip, Roller Bar & Plate - for Pressure Vessels & General Purpose ASTM B96/B96M, for Pressure Vessels & General Purpose ASME SB96; Strip – SAE J463, SAE J461; Studs – ASTM F468; Tube – MILITARY MIL-T-8231; Wire – ASTM B99/B99M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.308 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 60.0 ksi
@Thickness 2.03 mm
Tensile Strength, Ultimate 43.0 ksi
@Thickness 2.03 mm
Elongation at Break 60 %
@Thickness 2.03 mm
Tensile Modulus 15000 ksi
Modulus of Rigidity 5600 ksi
Poissons Ratio 0.34Calculated
Machinability 30 %
Forgeability 40 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000250 ohm-cm7% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 21.0 BTU-in/hr-ft²-°F
Melting Point 1780 - 1880 °F
Solidus 1780 °F
Liquidus 1880 °F
Annealing Point 900 - 1300 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1300 - 1600 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 92 - 96.7 %As Balance
Iron, Fe <= 0.80 %
Lead, Pb <= 0.050 %
Manganese, Mn 0.50 - 1.3 %
Nickel, Ni <= 0.60 %
Silicon, Si 2.8 - 3.8 %
Zinc, Zn <= 1.5 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC65500x1 / 293059

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.