MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bostik Big Tile & Stone™ Latex-Modified Mortar
Categories: Other Engineering Material

Material Notes: Description: Big Tile & Stone™ is a latex-modified, medium bed mortar used for interior or exterior installations to set all large sized ceramic, porcelain, granite, slate, marble, limestone, and dimension stone tiles. Use over properly prepared concrete; structurally-sound, exterior grade plywood (interior/dry use only); cementitious backer board; Bostik® Ultra-Set® Advanced; Bostik® Black-Top™; Bostik® GoldPlus™; and existing, well-bonded vinyl/VCT or ceramic tile. Big Tile & Stone may also be used as a leveling bed to compensate for uneven tile and stone thickness; smooth irregular or uneven substrates; or to minimize lippage.

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 3400 psi
@Time 2.42e+6 sec
Shear Strength 250 psi
@Time 2.42e+6 sec
Quarry to Wood; ANSI REQ 150
 300 psi
@Time 2.42e+6 sec
Quarry Tile
 375 psi
@Time 2.42e+6 sec
Porcelain Tile; ANSI REQ 200
 557 psi
@Time 2.42e+6 sec
Glazed Wall Tile; ANSI REQ 300
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 - 10.0 hourInitial Set
 10.0 - 15.0 hourFinal Set
Pot Life 60.0 - 120 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bostik Tube & Tile Caulk Siliconized-Acrylic Caulk
Bostik Professional Grade™ Ceramic Tile Mastic
Bostik Glass-Mate™ Glass Tile Mortar
Bostik D-2001® Ultra-Premium™ Ceramic Tile Mastic
MarkeTech Repton 868 Zirconia + 8 mol% Yttria (YSZ)

PBOSTK019 / 191555

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.