MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
The Chemical Company ChemFlexx™ DOA C22H42O4
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemflexx DOA is a Dioctyl adipate (DOA) plasticizer. DOA is an ester of 2-ethylhexanol and adipic acid. It is a low-toxicity, biodegradable, light colored, oily liquid generally used as a plasticizer for PVC. The compound is sometimes blended with other plasticizers such as DOP and DOTP. Chemflexx DOA features flexibility at low temperatures, good electrical properties, resistance to weathering, and good stability to heat. The product is used to manufacture clear food packaging films, children's toys, wire and cable.
Molecular Formula: C22H42O4

Information provided by The Chemical Company

Key Words: Dioctyl Adipate;Di-2-ethylhexyl adipate;DEHA;CAS Number 103-23-1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.925 - 0.929 g/cc
@Temperature 20.0 °C
Brookfield Viscosity 12.96 cP
@Temperature 68.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.010parent acid %
 
Thermal PropertiesOriginal ValueComments
Flash Point 206 °C
 242 °Cfire point
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %Weight percent
 
Descriptive Properties
Alcohol Content< 100ppm
AppearanceClear and free of suspended matter
Assay> 99.5%
Hazen Color Value (pt-co)< 15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTCC004 / 106993

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.