MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Envalior Pocan® S 1506 901510 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: PBT, injection molding grade, non-reinforced, elastomer-modified, high impact strength, even at low temperatures

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 g/ccISO 60
Density 1.22 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %50% RH; ISO 62
Water Absorption at Saturation 0.40 %ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm150x105x3; 260 °C / MT 80 °C; 600 bar; ISO 2577
Linear Mold Shrinkage, Transverse 0.018 cm/cm150x105x3; 260 °C / MT 80 °C; 600 bar; ISO 2577
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 70.0 MPaISO 2093-1
Tensile Strength, Yield 35.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield 4.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 1700 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 55.0 MPa2 mm/min; ISO 178-A
Flexural Yield Strength 45.0 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 1600 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 5.5 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) 20.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 75.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ISO 180-1U
 NB
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1eU
 NB
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched 25.0 kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
 75.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.1
@Frequency 1e+6 Hz
IEC 60250
 3.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.0020
@Frequency 100 Hz
IEC 60250
 0.017
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 600 VSolution B; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 130 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 130 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Thermal Conductivity 0.220 W/m-KISO 8302
Melting Point 225 °C10°C/min; ISO 11357-1,-3
Hot Ball Pressure Test 180 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 100 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO 75-1,-2
Vicat Softening Point 130 °C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 0.800 mm
Oxygen Index 22 %Method A; ISO 4589-2
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
IEC 60695-2-12
Shrinkage, MD 0.50 %
@Treatment Temp. 120 °C,
Time 14400 sec
Flow Direction Post-Molding, 150x105x3; ISO 294-4
Shrinkage, TD 0.50 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Molding, 150x105x3; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °Cinjection molding; ISO 294
 250 - 270 °C
Mold Temperature 80.0 °Cinjection molding; ISO 294
 80.0 - 100 °C
Drying Temperature 120 °C
Dry Time 4.00 - 8.00 hour
Moisture Content 0.00 - 0.020 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANW9195 / 208459

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.