MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyrocks Chemical 6001RM10 LDPE master batch
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: (MG70)=1:10

6001RM10 is flame retardant PE master batches bromine and antimony as flame retardant elements, carbonize and halogen-antimony synergistic mechanism play the flame retardant performance. 6001RM10 is PE resin as carrier, of high concentration flame retardant master batches, with good flammability, and no need to add other additives, adding a certain percentage of master batches to LDPE resin can extrusion granules directly. It meets the requirements of RoHS?SVHC?PFOS & PFOA?17P?PAHs...etc. 6001RM10 has characteristics of good flowability and processability, no dust pollution, easy to dye.

Information provided by Polyrocks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 8.00 MPaASTM D638
Elongation at Break 100 %ASTM D638
Flexural Strength 7.00 MPaASTM D790
Flexural Modulus 130 MPaASTM D790
Izod Impact, Notched 250 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-2
@Thickness 0.750 mm
 V-2
@Thickness 1.50 mm
 V-2
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 180 °CInjection Temperature
Mold Temperature 40.0 - 70.0 °C
 
Descriptive Properties
Injection Speed50-80%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPROCKS034 / 278542

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.