MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Premix Thermoplastics PREWHITE PE 13-60
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: PREWHITE PE 13-60 is a PE-LD based white masterbatch, developed especially for medical packages made by injection or blow molding of PE-LD, PE-LLD or PE-HD.

Due to the good dispersion PREWHITE PE 13-60 is well suited for very thin products.

According to FDA and BgVV regulations PREWHITE PE 13-60 is approved for use in contact with foodstuffs without limitations and also fulfills the requirements mentioned in U.S.P. XXII pages 1497-1500, 1572-1573. PREWHITE PE 13-60 carries the DMF number of 10333, Type III of FDA.

Information provided by Premix Thermoplastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/cc
Additive Loading 60 %TiO2 (rutile)
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.15 %When Produced
Shelf Life 12.0 MonthNormal Storing Conditions
 
Descriptive Properties
AppearanceGranule
CarrierPE-LD
Dosing, %0.5 to 30Depending on desired opacity
Light Fastness8-Very Good

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPREMA105 / 58120

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.