MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE RV-2250D BLK 111 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink RV-2250D BLK 111 is a high performance thermoplastic elastomer used in a variety transportation applications. Sarlink RV-2250D BLK 111 is a high hardness, medium density extrusion grade that exhibits sunlight resistance and UV characteristics.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; Light Stabilized; Medium Density; Low Flow; High Hardness; Sunlight Resistant; UV Absorbing

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Viscosity 545 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50
@Time 15.0 sec
Injection Molded; ISO 868
 51
@Time 5.00 sec
Injection Molded; ISO 868
 54
@Time 1.00 sec
Injection Molded; ISO 868
 54.5
@Treatment Temp. 110 °C,
Time 15.0 sec
Change in Air, 1008 hr; ISO 888
 55.4
@Treatment Temp. 110 °C,
Time 5.00 sec
Change in Air, 1008 hr; ISO 888
 55.9
@Treatment Temp. 125 °C,
Time 15.0 sec
Change in Air, 168 hr; ISO 888
 56.5
@Treatment Temp. 125 °C,
Time 5.00 sec
Change in Air, 168 hr; ISO 888
 58.4
@Treatment Temp. 110 °C,
Time 1.00 sec
Change in Air, 1008 hr; ISO 888
 59.2
@Treatment Temp. 125 °C,
Time 1.00 sec
Change in Air, 168 hr; ISO 888
Tensile Strength at Break 1830 psiAcross Flow, Type 1, 20 in/min; ISO 37
 2200 psiFlow, Type 1, 20 in/min; ISO 37
 268 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 288 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 1830 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
 1840 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 1470 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 2050 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 1730 psi
@Strain 100 %,
Treatment Temp. 125 °C
Across Flow, Type 1, Change in Air, 6.61 in; ISO 188
 1760 psi
@Strain 100 %,
Treatment Temp. 110 °C
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 2640 psi
@Strain 100 %,
Treatment Temp. 110 °C
Flow, Type 1, Change in Air, 1008 hr; ISO 188
 2890 psi
@Strain 100 %,
Treatment Temp. 125 °C
Flow, Type 1, Change in Air, 168 hr; ISO 188
Elongation at Break 360 %Flow, Type 1, 20 in/min; ISO 37
 720 %Across Flow, Type 1, 20 in/min; ISO 37
 184 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 468 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
 504 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 500 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
 830 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
Compression Set 46 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ISO 815
 75 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ISO 815
 85 %
@Temperature 90.0 °C,
Time 252000 sec
Type 1; ISO 815
 100 %
@Temperature 125 °C,
Time 252000 sec
Type 1; ISO 815
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 410 °F
Middle Barrel Temperature 400 - 420 °F
Front Barrel Temperature 410 - 430 °F
Nozzle Temperature 420 - 440 °F
Melt Temperature 420 - 440 °F
Mold Temperature 95.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 120 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® TPE RV-2235B Thermoplastic Elastomer
Radici Raditer® B RV 100 Polybutylene Terephthalate with 10% Glass fiber

PTEKNQ1126 / 237617

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.