MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
General Industrial Polymers ANIONIC LATEX LTX 6A Styrene-Butadiene Copolymer Latex
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Latex LTX 6A is an aqueous dispersion with high content of solids of a butadiene-styrene copolymer produced by cold emulsion polymerization, using a fatty soap as an emulsifier. It has approximately 24% of bound styrene in the copolymer. The product is protected with a biocide to avoid bacterial contamination.

CAS No.: 9003-55-8.

Supply Form Viscous white liquid

Use: Latex LTX 6A is used in the production of gel and non-gel laminated foam, molded foam, lining impregnation, carpet backing, agglomerates of coconut fiber and cork, manufacture of insoles, water base adhesives compositions and in modification of asphalt emulsions.

Information provided by General Industrail Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 68 %ASTM D1417
pH 11ASTM D1417
Brookfield Viscosity 800 cPRVT, spindle 2, 20 rpm; ASTM D1417
Mooney Viscosity 135[ME]; ASTM D1646
Surface Tension 33.5 dynes/cmASTM D1417
 
Chemical PropertiesOriginal ValueComments
Styrene Content 24 %Bound; ASTM D5775

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGENIND010 / 294799

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.