Specimens for property data below were 25-75 mm diameter The high nickel content of this electrode provides excellent resistance to heat and scale at temperatures above 1800°F, leading to uses such as heat exchangers and radiant tubes. Alloy 330 electrodes are also used for repair of defects in castings of the 330 analysis. |
UNS N08330, AMS 5592, AMS 5716, ASTM B511, ASTM B512, ASTM B535, ASTM B536, ASTM B546, SAE J405 (30330), SAE J412 (30330); RA330 |