MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-FR-TPEE Non-halogen TPEE (Hytrel) Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: TPEE(Thermoplastic Polyester Elastomer)is a block polymer which contains polyester hard segment and polyether soft segment. Polyether soft segment and noncrystalline polyester formation of amorphous polyester hard segment crystalline into micro region which make physical cross-linking point. TPEE is manufactured 1,4-butanediol (1,4-Butylene glycol) and poly-butylene glycol (Polytetramethylene glycol) and terephthalate (DMT) or terephthalic acid (PTA) for the condensation-copolymerization,and it is made by thermoplastic polyester elastomer composites via kneading program. Due to shortcoming for the structure of TPEE is flammable, especially the limited use for the ingredients of polyester and polyether soft segment and alcohols and esters of TPEE. Therefore, GYC technology department developed environmental friendly flame retardant GY-FR-TPEE for TPEE. When the GY-FR-TPEE added to TPEE, it will have fire retardant effect for rubber elasticity and the strength of fire retardant engineering plastics; Soft segment gives it elasticity fireproof structure, so there is resistance rubber TPEE all properties; Hard segment given Its processing performance, so there TPEE plastic fire performance; and rubber, it has a better processing performance and longer service life and fire protection; and engineering plastics compared to the same high fire intensity features, and flexibility and dynamic mechanical properties better. GY-FRTPEE enhances the added value of TPEE, and makes it have more superior fire properties. TPEE with flame retardant widely used in fire retardant wire and fiber coated housing and a variety of flameproof electrical appliances and automotive parts.

Advantages:

  • Excellent flame retardant properties
  • Thermal decomposition temperature (resistant to 300 ° C processing temperature)
  • Injection grade and extrusion grade of flame retardant TPEE
  • Long time flame retardant effect
  • Electric particularly good, suitable for a variety of electronic products
  • High stability
  • Environmental non-halogen products
  • good dispersion with TPEE elastomers (Compound)
  • Excellent voltage resistance characteristics
  • Very low coefficient of smoke
  • Improve TPEE elastomer oxygen index (LOI)
Applications:
  • Automotive Parts retardant Applications: spring, wire inside and outside the skin, ball joints bushings, bumpers, seat belt buckle housing, joystick housing
  • Mechanical parts retardant Applications: flexible joints, Vbelt, the belt, all kinds of pipes (such as hydraulic tube)
  • Motor, communication materials fire retardant
  • Applications: telephone cable jacket, the fiber coating, gears, cams, etc.
  • Other high-priced electronic / wire / cable and other products flame-retardant applications

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature >= 300 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.50 %
 
Descriptive Properties
AppearanceSolid fine powder
ColorWhite
Purity100%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN190 / 266498

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.