Characterization: Baytec SPR-186A is a two-component 100%-solids spray system with a Shore A hardness of 86*. Properties / Applications: Baytec SPR-186A is a two-component 100%-solids spray system with a Shore A hardness of 86*. The isocyanate component is a modified diphenylmethane diisocyanate (MDI) qusi-prepolymer and the polyol component is a polyether blend. The system can be pigmented to most any color. As with any product, use of the Baytec SPR-186A in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability. Information provided by Covestro |